Aluminum profile extrusion press machine spare part billet container

Aluminum profile extrusion press machine spare part billet container

Delivery time: 15 days

Aluminum profile extrusion press machine spare part billet container.

Heating the extrusion container: After a new extrusion container is assembled, it must be heated from a cold state to the operating temperature. To avoid thermal stresses caused by uneven heating—which could lead to cracking or even structural failure—gradient heating is required; the heating schedule is provided as below:

Heating temperature/ ℃200250300350400420
Holding time / h44~66~88~1010~1212~14